Ensayo a compresion de probetas ASTM C39
Determination of Compression Strength in Concrete Cylinders
Overview of the Testing Procedure
- The video demonstrates the determination of compression strength in cylindrical concrete specimens, whether molded or extracted cores, following STMS 39 standards.
- It specifies that the standard applies to concrete with a unit weight exceeding 800 kg/m³ and outlines necessary equipment such as metal squares for checking perpendicularity.
- Graduated sheets are used to check flatness and depressions on the specimen's surfaces; a micrometer screw gauge measures cylinder diameter with an accuracy of ±0.25 mm.
Preparation and Measurement Requirements
- The testing procedure begins immediately after removing the specimen from curing conditions while maintaining moisture; two diameters must be measured at right angles mid-height.
- Specimens not meeting dimensional criteria (more than 2% difference in diameter or misalignment beyond specified limits) will not be tested; polishing may be required for non-compliant ends.
Testing Execution Steps
- Clean both upper and lower press supports before placing the specimen; align it centrally with the pushing block and ensure load indicator reads zero before applying load continuously without impact.
- During loading, maintain a constant application speed (±0.05 MPa/s); record maximum load supported by the specimen until it fails, noting fracture type and concrete appearance for analysis.